logo-robert-laminage-large-white

 

Engineered metals
for precision industries

Data sheet - Hastelloy C-276

www.robertlaminage.com

Hastelloy C-276
NiMo16Cr15W

Ni51-63Mo15-17Cr15-16.5Fe4-7W3-4.5

Chemical composition

Ni51-63

P0.02 max

Fe4-7

Mn1 max

Si0.08 max

S0.01 max

Co2.5 max

C0.01 max

Mo15-17

Cr15-16.5

OtherW 3-4.5 / V 0.3 max

Alloy name
RLSA no.986
EN standardNiMo16Cr15W
DIN standard2.4819
UNS no.*N10276

*Unified Numbering System (USA)

Characteristics and main uses

Hastelloy C-276 is a nickel-chrome-molybdenum alloy with tungsten. It is characterized by:

  • Extraordinary resistance across a wide range of corrosive, watery media; in particular oxidizing and reducing acids
  • Particularly high resistance against chloride-induced crevice, pitting and stress corrosion

Main uses

Hastelloy C-276 can be used in many chemical processes with both oxidizing as well as reducing media. The high chrome and molybdenum concentrations make the alloy resistant to chloride ion attacks. The tungsten content further increases this resistance. Hastelloy C-276 is one of the few materials that are resistant against chlorine gas, hypo-chlorite and chlorine dioxide solutions. The alloy is characterized by excellent resistance against concentrated solutions of oxidizing salts (such as iron III and copper chloride).

Hastelloy C-276 has a broad field of application in the chemicals and petrochemicals industry, for components in organic processes containing chlorides, and for catalytic systems. The material can be used especially in cases where hot, contaminated mineral acids, solutions or organic acids (such as formic acid and acetic acid) and sea water occur.

  • Examples of fields of application:
  • Paper and pulp industry, e.g. for digestion and bleaching tanks
  • Washers, agitators and wet ventilators in flue gas desulfurization systems
  • Equipment and components for acid gas applications
  • Reactors for acetic acid production
  • Sulfuric acid coolers
  • Methylene diphenyl isocyanate (MDI)
  • Manufacturing and processing of contaminated phosphoric acid

Physical properties Units
Density (20°C) 8.89 Kg/dm³
Melting point 1325-1370 °C
Longitudinal elasticity modulus 208-143 (20-1000°C) GPa
Thermal conductivity W/m·K
Electrical conductivity m/Ω·mm²
Electrical resistivity µΩ·m
Linear expansion Coefficient 10⁻⁶·K⁻¹
IACS (International Annealed Copper Standard) %
Poisson's ratio
Capabilities
Corrosion resistance4 sauf acide nitrique
Hot deformation
Cold deformation
Electrodepositing
Diamond cutting
Nitriding
Mechanical polishing
Welding without filler3
Brazing

1 poor | 2 average | 3 good | 4 very good | - no info

Heat Treatment / Hardening
Annealing temperature 1100-1160 °C
Temperature for stress relief treatment °C
Hardening temperature °C
Hardening treatment time hour(s)

Alloy mechanical properties

Hastelloy C-276
Possible hardness range 250 Min HV
Possible Rm range 730 Min MPa

Non-exhaustive list of grades

Grade According to standard Hardness
(HV: Vickers)
min - max
Rm
(MPa)
min - max
Rp 0.2
(MPa)
min - max
Elongation
(%) where L0 = 100mm
min - max
L0 Grain size
(µm)
min - max

Do not hesitate to ask us for your specific grades and parameters. We can make productions according to your needs.

Contact us

Do not hesitate to contact us for a quote, any questions or advice. We will get back to you as soon as possible. 

Your request
Quote request
mm
mm
mm
mm
mm
mm
kg
HV
HV
Surface condition measurement
µm
µm
µm
µm
Coil diameter
mm
mm
mm
Packaging
EN10204 certificate
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.