ROBERT 32
INOX
Fe reste Cr16.40 Ni6.5 C0.11
Chemical composition |
---|
Cu1 max
Ni6.4-6.6
P0.04 max
FeBAL
Mn1-1.4
Si1-1.3
S0.008 max
C0.10-0.12
Mo0.6-0.8
Cr16.20-16.60
OtherN 0.11 max
Alloy name | |
---|---|
RLSA no. | 962 |
EN standard | |
DIN standard | 1.4310 (+C) |
UNS no.* | S30100 |
*Unified Numbering System (USA)
Characteristics and main uses
1.4310 avec amélioration de la résistance à la fatigue
Physical properties | Units | |
---|---|---|
Density (20°C) | 7,90 | Kg/dm³ |
Melting point | 1400-1425 | °C |
Longitudinal elasticity modulus | GPa | |
Thermal conductivity | W/m·K | |
Electrical conductivity | m/Ω·mm² | |
Electrical resistivity | µΩ·m | |
Linear expansion Coefficient | 10⁻⁶·K⁻¹ | |
IACS (International Annealed Copper Standard) | % | |
Poisson's ratio | 0,29 |
Capabilities | |
---|---|
Corrosion resistance | 3 |
Hot deformation | |
Cold deformation | |
Electrodepositing | |
Diamond cutting | |
Nitriding | |
Mechanical polishing | |
Welding without filler | |
Brazing |
1 poor | 2 average | 3 good | 4 very good | - no info