logo-robert-laminage-large-white

 

Engineered metals
for precision industries

Data sheet - Cu OFE

www.robertlaminage.com

Cu OFE
CUIVRE - CuC2

Cu>99.99 O0.0005max

Chemical composition

Cu99.99

Pb0.005 max

O0.0005 max

Alloy name
RLSA no.120
EN standardCW009A
DIN standard
UNS no.*C10100

*Unified Numbering System (USA)

Characteristics and main uses

Cu-OFE is a high conductivity oxygen-free copper with a minimum of 99.99% Cu. It offers the advantages of hard pitch electrolytic copper (ETP) and phosphorus deoxidized copper. High purity with less than 5 ppm oxygen and absence of deoxidizers represents a minimum electrical conductivity of 101% of IACS as well as no susceptibility to hydrogen embrittlement. Cu-OFE has very good formability and can be brazed and welded, making it superior to Cu-ETP in these aspects.
The main areas of application are electrical, electronic and communication components as well as vacuum technology.

CU-OFE copper is resistant to natural and industrial atmospheres as well as maritime air, drinking and service water, non-oxidizing acids, alkaline solutions and neutral salt solutions.
Copper is not resistant to ammonia, halide, cyanide and hydrogen sulfide solutions and atmospheres, oxidizing acids and sea water (especially at high flow rates).

 

Main uses

Radar components, electrical engineering components, conductors, contacts and terminals, printed circuits and flexible circuits

Physical properties Units
Density (20°C) 8,94 Kg/dm³
Melting point 1083 °C
Longitudinal elasticity modulus 127 GPa
Thermal conductivity W/m·K
Electrical conductivity 58 m/Ω·mm²
Electrical resistivity <0.017241 µΩ·m
Linear expansion Coefficient 17 10⁻⁶·K⁻¹
IACS (International Annealed Copper Standard) 100 %
Poisson's ratio
Capabilities
Corrosion resistance4
Hot deformation3
Cold deformation4
Electrodepositing4
Diamond cutting
Nitriding
Mechanical polishing3
Welding without filler3
Brazing4

1 poor | 2 average | 3 good | 4 very good | - no info

Heat Treatment / Hardening
Annealing temperature 350 °C
Temperature for stress relief treatment 150-200 °C
Hardening temperature °C
Hardening treatment time hour(s)

Comments on heat treatments

The electrical conductivity depends on chemical composition, the level of cold deformation and the grain size. A high level of deformation as well as a small grain size decrease the conductivity

Alloy mechanical properties

Cu OFE
Possible hardness range 75 - 125 HV
Possible Rm range 225 - 360 MPa

Non-exhaustive list of grades

Grade According to standard Hardness
(HV: Vickers)
min - max
Rm
(MPa)
min - max
Rp 0.2
(MPa)
min - max
Elongation
(%) where L0 = 100mm
min - max
L0 Grain size
(µm)
min - max
R200 40 - 65* 200 - 250 ≤ 100* ≥ 42 50
R220 40 - 65* 220 - 260 ≤ 140* ≥ 33 50
R240 65 - 95* 240 - 300 ≥ 180 ≥ 8 50
R290 90 - 110* 290 - 360 ≥ 250 ≥ 4 50
R360 ≥ 110* ≥ 360 ≥ 320 ≥ 2 50

Do not hesitate to ask us for your specific grades and parameters. We can make productions according to your needs.

Contact us

Do not hesitate to contact us for a quote, any questions or advice. We will get back to you as soon as possible. 

Your request
Quote request
mm
mm
mm
mm
mm
mm
kg
HV
HV
Surface condition measurement